PCBA and EMS

Conformal Coating in China

An acrylic, urethane, silicone or parylene film applied over an assembled board. Protection depends on chemistry, thickness, cure and masking, and each is inspectable.

Conformal Coating: recorded factories

Ordered by evidence strength, then by most recent review. Each profile states what was checked, on what date, and which processes are subcontracted rather than performed on site. A listing is not a guarantee of factory ownership or certification validity.

SEIC (Shenzhen Shinelong Electronics)

深圳先隆电子实业有限公司

SEIC pages say 75, 400 or 500 staff and put the plant at 1,800 or 12,000 square metres. A buyer's question list built from the differences.

Shenzhen

Founded 1997 · Evidence: Public sources reviewed · Reviewed 2026-11-19

View factory profile

King Brother (KINGBROTHER)

深圳市金百泽电子科技股份有限公司

Kingbrother books 100,000 PCB part numbers a year, while an older page on the same site implies 120,000. Neither figure is in square metres.

Shenzhen rigidmultilayer

Founded 1997 · Evidence: Public sources reviewed · Reviewed 2026-11-11

View factory profile

What this service covers

Conformal coating applies a thin polymer film over an assembled board to protect against moisture, contamination and, in some cases, mechanical abrasion. Four chemistries dominate:

  • Acrylic (AR) is the default: cheap, easy to apply, easy to remove for rework, and the weakest against solvents.
  • Polyurethane (UR) resists solvents and abrasion better and is harder to rework.
  • Silicone (SR) stays flexible across a wide temperature range, which matters for boards that see thermal cycling or vibration.
  • Parylene (XY) is applied by vapour deposition in a vacuum chamber, gives the most uniform thin film, and requires the most masking because it coats everything.

IPC-CC-830 is the qualification standard for the coating material, and it is a separate question from whether the application on your board is correct.

What decides whether the coating protects anything

  • Surface cleanliness before coating. Coating over flux residue traps contamination and can accelerate electrochemical failure rather than prevent it. The cleaning step is part of the process, not an optional extra.
  • Thickness, measured in the right place. A nominal figure means little without a measurement location. Coating thins over edges and tall components and pools in valleys.
  • Masking definition. Connectors, test points, pressure sensors, relays and anything that must make electrical contact have to be masked. A missing mask is a functional failure, not a cosmetic one.
  • Cure method. Room-temperature cure, oven cure and UV cure produce different film properties. UV-cure coatings need line of sight, so shadowed areas stay uncured unless they are also moisture-cured.
  • Inspection. UV tracer in the coating makes coverage visible under black light. That is how a coating line checks its own work, and a supplier without it is inspecting by eye.

What drives the price

  • Board area and coating thickness, which set material consumption.
  • Masking complexity. Masking is manual labour and it is usually the largest cost on a small batch.
  • Application method: manual spray, selective coating machine, dip, or vacuum deposition.
  • Cure time and rework, since some chemistries cannot be reworked without removing the whole film.
  • Inspection requirement, including thickness measurement and UV coverage check.

What we check before listing a factory here

  • The factory states which chemistries it applies and whether it subcontracts parylene, which needs a vacuum chamber most sites do not have.
  • Cleaning before coating is part of the process flow, and the compatibility with the flux used at assembly is stated.
  • Thickness is measured and recorded, with the measurement location defined.
  • Masking is documented per assembly with a mask drawing, not decided by the operator.
  • UV inspection is used, or the factory states how coverage is verified without it.
  • Rework and repair of a coated board is either offered or explicitly excluded, because removing a cured coating is a separate capability.

Where it goes wrong

  • Coating over an unclean board. Residue is sealed in, and the failure appears as dendrite growth months later.
  • Connector masked with tape and the tape left in place. The unit passes and the connector fails at first mating.
  • Thickness quoted from the material datasheet. The datasheet describes the cured film, not the film on your board’s edge.
  • Cure checked by touch. A tacky film that feels dry can still be under-cured, and adhesion fails later.
  • Rework after coating without recoating. The repair area is left unprotected and becomes the first failure site.

How it differs from neighbouring services

Coating follows assembly and cleaning. It is not a substitute for a clean process, and it does not protect a joint that was already defective. Repair and rework after coating is a separate service, because the film has to be removed first.

What to send in an RFQ

The assembly drawing with keep-out and masking areas, the required chemistry and thickness standard, the operating environment, the cleaning requirement, and whether rework access is needed later. The conformal coating quote specification lists the fields that change the price.

If the board is going into a humid or condensing environment, read environmental compliance before choosing a chemistry; the choice depends on the failure mode you are protecting against.