Soldering Explained
Soldering as a process: reflow profiles, wave and selective soldering, hand rework and what a profile record proves about a production lot.
Questions this topic answers
Short answers first. Each one is written to be quoted on its own, and each one says what has to be on record before the answer can be trusted.
- 01
What should a reflow profile record show?
The board revision, thermocouple positions, ramp rate, time above liquidus, peak temperature and cooling rate. A curve with no board identity cannot be matched to your order, and a peak temperature without a location on the board is only half a record.
- 02
When is selective soldering needed?
When a board has through-hole parts that cannot tolerate a full wave pass or when the layout puts heat-sensitive parts near the solder side. The process is slower and needs its own program, so it should be identified at quote stage rather than added later.
- 03
How is hand soldering controlled in production?
By defining which joints may be touched, the maximum contact time and the inspection after each repair. Without those limits, hand work becomes an invisible process. Ask for the count of hand-touched joints per board in a sample lot.
- 04
Does a clean-looking joint mean the process was in control?
No. Appearance misses cold joints under large packages and heat damage inside components. Combine visual inspection with the profile record and, where the design needs it, cross-section or X-ray evidence tied to your lot.
Where this meets the directory
These pages answer the commercial question — who can do the work and what is on record. This topic answers the technical question behind it.
Articles filed here
The four questions above are the standing brief for this topic. Dated field notes are published at the blog index as each one is finished.